Customization: | Available |
---|---|
Standard: | JIS, GB, DIN, BS, ASTM, AISI |
Application: | Loader, Construction Machinery, Metallurgical Machinery, Cement Plant, Mining Machine, Thermal Power Plant, Coal Yard |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Forged Grinding Media Ball/Grinding Media for Mine
DESCRIPTION
1. Grade: Explore the pinnacle of adaptability with our extensive selection of grades including B2, B3, 45#, 50Mn, 60Mn, 65Mn, B2, B3, B6, BU. Each one is expertly engineered to fulfill your tailored needs with precision and excellence.
2. Diameter: Choose from our vast array of grinding media balls, ranging from 20mm to 150mm in diameter. This extensive range offers unparalleled precision and versatility for all your application requirements.
3. Hardness: Engineered for resilience, our balls boast a formidable hardness of 55-65HRC, ensuring they endure through the toughest conditions and maintain their durability over time.
4. Breakage Rate: Experience unrivaled reliability with a breakage rate of less than 1%, promising continuous and dependable operation.
5. Impact Value: With a remarkable impact value exceeding 12j/Cm^2, our grinding media balls are designed to withstand even the most strenuous impacts.
6. Endurance impact test times: Our media balls have been rigorously tested for endurance, surpassing 20,000 impact cycles, ensuring sustained superior performance.
7. Uniform hardness, high wear resistance, high impact value: Crafted for excellence, our product ensures uniform hardness, superior wear resistance, and an exceptional impact value.
Forged Grinding Media Steel Ball Chemical Composition:
Materials | C% | Si% | Mn% | P% | S% | Cr% |
B2 | 0.70-0.85 | 0.17-0.37 | 0.70-1.00 | ≤0.035 | ≤0.035 | 0.4-0.6 |
B2-1 | 0.55-0.70 | 0.15-0.30 | 0.65-0.85 | ≤0.020 | ≤0.020 | 0.70-1.10 |
High Carbon B2 | 0.85-1.10 | 0.15-0.45 | 0.40-1.20 | ≤0.035 | ≤0.035 | 0.20-1.10 |
B3 | 0.58-0.66 | 1.70-1.90 | 0.68-0.80 | ≤0.030 | ≤0.030 | 0.78-0.90 |
45# | 0.42-0.50 | 0.17-0.37 | 0.5-0.8 | ≤0.035 | ≤0.035 | 0.25max |
B4 | 0.65-0.75 | 1.20-1.40 | 0.50-0.70 | ≤0.025 | ≤0.025 | 0.85-1.00 |
B6 | 0.75-0.90 | 0.17-0.37 | 0.8-1.02 | ≤0.035 | ≤0.035 | 0.88-0.98 |
B6-1 | 0.82-0.90 | 0.15-0.35 | 0.90-1.05 | ≤0.020 | ≤0.020 | 0.88-0.98 |
BU | 0.95-1.05 | 0.15-0.35 | 0.95-1.05 | ≤0.025 | ≤0.025 | 0.45-0.55 |
1090 | 0.90-1.10 | 0.17-0.37 | 0.60-0.90 | ≤0.025 | ≤0.025 | ≤0.025 |
42CrMo | 0.38-0.45 | 0.20-0.40 | 0.50-0.80 | ≤0.035 | ≤0.035 | 0.90-1.20 |
40Cr | 0.37-0.45 | 0.20-0.40 | 0.50-0.80 | ≤0.035 | ≤0.035 | 0.80-1.10 |
65MN | 0.62-0.70 | 0.17-0.37 | 0.90-1.20 | ≤0.035 | ≤0.035 | ≤0.25 |
60MN | 0.57-0.65 | 0.17-0.37 | 0.70-1.00 | ≤0.035 | ≤0.035 | ≤0.25 |
50MN | 0.48-0.56 | 0.17-0.37 | 0.70-1.00 | ≤0.035 | ≤0.035 | ≤0.25 |
Diameter(mm) | Diameter Tolerance(mm) | Surface Hardness(HRC) | Impact Toughness(j/cm2) |
Φ20 | +2, -1 | >60HRC | ≥12j/cm2 |
Φ25 | |||
Φ30 | |||
Φ40 | |||
Φ50 | |||
Φ60 | +3, -2 | ||
Φ70 | |||
Φ80 | |||
Φ90 | |||
Φ100 | +4, -2 | ||
Φ110 |
|||
Φ120 |
>58HRC | ||
Φ130 |
|||
Φ140 |
+4, -3 | >55HRC |